1. Environmental protection(Can almost reach the edible level)
2. High glossy and super coating performance
3. Low unit coating area
Product Performance |
Water-Based UV Varnish |
Conventional products |
||
Oil UV Varnish |
Old Water-Based Varnish |
Laminating |
||
Environmental Protection |
By the SGS testing and animal toxicity testing. Can almost reach the edible level |
Contain highly toxic toluene. With TP, TM, and other carcinogenic substances |
Ethylene glycol monobutyl ether (reproductive toxicity) |
Glues are highly toxic, |
paper can not be recycled. |
||||
Odor |
Crude oil can only smell a bit of alcohol, but the coated paper completely odor-free. |
Crude oil has strong odor, the coating paper has a very strong initiator and toluene odor |
The smell of ethylene glycol monobutyl ether (reproductive toxicity), and ammonia odor |
Strong smell of glue (toluene) |
Glossiness |
Up to 98,most of the region can almost reach 90 |
10 less than water based UV Varnish for everage |
40-50 |
Can reach more than 90 |
Abrasion Resistance |
Four pounds pressure conditions,500 times |
Four pounds pressure conditions, Around 100 times |
Lower than the oil UV Varnish |
Well |
Toughness
- fold test |
The coating will not crack or peel off at the folding place |
Crack, peel off |
Not peel off |
At the folded place, film will peeled off from the paper |
Adhesion
- the tape test |
With adhesive tape on paper, the coating will not peel from the paper. |
Normally will peel |
Usually will peel,a little better than oil |
Good |
Water Permeability |
Impermeable, meet water resistance standards test. |
Impermeable |
Permeate Immediately |
Impermeable |
Levelling Property |
Can reach the laminating effect |
Can see pigskin grain with naked eye |
Slightly better than the oil |
Good |
Curing Speed |
Energy density: 8mj/cm2 (Levelling channel is not less than 2 meters) |
The same as Water Based UV Varnish |
Difficult to dry, need baking |
Appearance |
micro-milky |
Viscosity |
12--18S (Cai’s 4# cup 25°C) |
Solid contents |
(40±3)% |
Wearing resistance |
≥200 times (4 pound /copy paper have not transparent decolouration) |